Effect of grinding aids and process parameters on dry fine grinding …
In the first dry grinding process, 4 g of the materials (PTFE and salt additive mixture) were ground in air. In the second washing step, 2 g of the ground sample was placed in a capped Erlenmeyer flask filled with 300 mL of water/ethane (50/50) solution and stirred for 4 h at room temperature on a magnetic stirring apparatus (524G, Meiyingpu ...